Atomic Layer Deposition in Energy Conversion Applications
Samenvatting
Combining the two topics for the first time, this book begins with an introduction to the recent challenges in energy conversion devices from a materials preparation perspective and how they can be overcome by using atomic layer deposition (ALD).